Search
+86-138-1482-9868 +86-512-65283666

Before you start shopping

We use first- and third-party cookies including other tracking technologies from third party publishers to give you the full functionality of our website, to customize your user experience, perform analytics and deliver personalized advertising on our websites, apps and newsletters across internet and via social media platforms. For that purpose, we collect information about user, browsing patterns and device.

By clicking "Accept All Cookies", you accept this, and agree that we share this information with third parties, such as our advertising partners. If you prefer, you can choose to continue with "Only Required Cookies". But keep in mind that blocking some types of cookies may impact how we can deliver tailored content that you might like.

For more information and to customize your options, click on "Cookie settings". If you want to learn more about cookies and why we use them, visit our Cookie Policy page at any time. Cookie Policy

Accept All Cookies Close

About Trojan

Founded in 2005, Trojan (Suzhou) material technology Co., Ltd is located in Suzhou City, Jiangsu Province. It is a professional Metallographic Cutting Accessories Suppliers in China, We have a strong production team, which can be processed according to product instructions or samples provided by customers. wholesale Cutting Accessories and other products. We have our own equipment, one-stop production, factory direct sales, high quality and low price. The company has passed ISO, CE and other system certifications, and its products are widely used in metallographic testing laboratories in various industries at home and abroad, and have been widely recognized by customers. As your trusted OEM/ODM Metallographic Cutting Accessories Company, in order to avoid undiscovered failures, we will perform 100% appearance and functional inspections on every detail before shipment to meet all your requirements for product quality. If you find any product defects, we are willing to negotiate a solution. Looking forward to cooperating with you!

news & exhibition

First-hand consultation you want to know

Industry knowledge

What are some essential metallographic cutting accessories used in sample preparation for microscopy analysis?

Abrasive Cut-off Wheels: These wheels, often made of diamond or silicon carbide, are used for cutting through various materials with precision. They provide controlled cutting and reduce heat generation, minimizing potential damage to the sample.
Cut-off Machines: These machines are specifically designed to hold the cutting wheels and provide a stable platform for cutting. They offer adjustable cutting parameters such as speed, feed rate, and cutting depth, ensuring consistent results.
Cooling Systems: Cooling systems, such as recirculating coolants, are vital to prevent overheating of both the sample and the cutting blade. This helps maintain the structural integrity of the sample and prolongs the life of the cutting accessories.
Mounting Presses: After cutting, samples are often encapsulated in a mounting material, such as epoxy resin. Mounting presses are used to apply pressure and heat to the mounting material, ensuring proper encapsulation and minimizing voids.
Grinding and Polishing Equipment: While not directly cutting accessories, grinding and polishing steps are integral to the sample preparation process. Equipment such as grinding machines and polishing cloths are used to refine the sample surface, removing cutting-induced damage and revealing the microstructure.
Sectioning Consumables: These include items like cutting blades, cutting lubricants, abrasive papers, and mounting resins. High-quality consumables are essential for achieving consistent and reproducible results in metallographic analysis.
Safety Equipment: Personal protective equipment (PPE) such as safety glasses, gloves, and lab coats are crucial when using metallographic cutting accessories to ensure the operator's safety.
Microscope Slides: Once the samples are prepared, they are often mounted on microscope slides for easy handling and analysis under a microscope.
Labeling and Documentation Tools: Properly labeling the prepared samples with information such as material type, cutting parameters, and orientation is essential for maintaining a comprehensive record and accurate analysis.
Microscopes: While not accessories for cutting, microscopes are used for the actual analysis of the prepared samples. They allow researchers to observe the microstructure of materials, identify features, and gather valuable information.

What factors should be considered when selecting metallographic cutting accessories for different types of materials?

Material Hardness: The hardness of the material to be cut is a key factor. Softer materials may require different cutting accessories compared to harder materials. For example, harder materials might necessitate diamond abrasive cut-off wheels for efficient cutting.
Material Composition: The composition of the material, including its chemical makeup and the presence of any inclusions or phases, can influence the choice of cutting accessories. Some materials might be more prone to chipping or damage during cutting due to variations in composition.
Sample Size and Shape: The size and shape of the sample play a role in selecting appropriate accessories. Irregularly shaped samples might require specialized clamping or holding mechanisms to ensure accurate cutting.
Sample Quantity: If multiple samples need to be prepared from the same material, considerations such as the longevity of cutting blades and consumables become important to maintain consistent results.
Surface Finish Requirements: Depending on the analysis goals, the required surface finish after cutting might vary. Some materials might need minimal post-cutting grinding and polishing, while others might require more extensive surface refinement.
Cooling Requirements: Some materials are more sensitive to heat generation during cutting. Heat can cause distortion, phase changes, or damage to the microstructure. In such cases, efficient cooling systems become crucial to maintain sample integrity.
Cutting Speed and Feed Rate: Different materials have optimal cutting parameters for achieving clean cuts without excessive damage. Selecting cutting accessories that allow adjustment of cutting speed and feed rate can help tailor the process to the material.
Cost Considerations: Different cutting accessories have varying costs. Balancing the cost of consumables and equipment against the quality of results and the specific needs of the analysis is important.
Safety: The safety of the operator is paramount. Some materials might produce hazardous dust or fumes during cutting, necessitating the use of appropriate ventilation systems and personal protective equipment.
Compatibility with Equipment: Ensure that the chosen cutting accessories are compatible with the equipment you have available, such as the type of cut-off machine and mounting press.
Expertise and Experience: The skill level of the operator also plays a role. Some cutting accessories require more advanced techniques and handling. Matching the equipment to the operator's expertise can lead to better results.
Analytical Goals: Consider the ultimate goal of the analysis. If specific features or microstructural details need to be observed, selecting cutting accessories that minimize damage and artifacts becomes crucial.