We use first- and third-party cookies including other tracking technologies from third party publishers to give you the full functionality of our website, to customize your user experience, perform analytics and deliver personalized advertising on our websites, apps and newsletters across internet and via social media platforms. For that purpose, we collect information about user, browsing patterns and device.

By clicking "Accept All Cookies", you accept this, and agree that we share this information with third parties, such as our advertising partners. If you prefer, you can choose to continue with "Only Required Cookies". But keep in mind that blocking some types of cookies may impact how we can deliver tailored content that you might like.

For more information and to customize your options, click on "Cookie settings". If you want to learn more about cookies and why we use them, visit our Cookie Policy page at any time. Cookie Policy

Accept All Cookies Close

Preparation of microstructure samples of ternary precursor powder for lithium-ion battery cathode materials

Under the dual pressures of energy shortage and global environmental protection, lithium batteries, with their high energy density and long cycle life, have become the core choice in the fields of energy storage and power. From power station energy storage systems, telecommunications and communication uninterruptible power supplies, to electric vehicles, military and aerospace equipment, the application scope of lithium batteries continues to expand.

In the composition of ternary lithium-ion batteries, the cathode material plays a decisive role in battery performance, and preparing high-quality ternary precursor powders is the key first step to obtain high-quality cathode materials. However, to accurately evaluate the quality and performance of ternary precursor powder, metallographic preparation is an indispensable key step. The following are the sample preparation method steps for your reference. 

① P2500 metallographic sandpaper grinding

② CS + 3μm PD-WT diamond polishing solution polishing

③ ZN + 0.05μm AO-W alumina polishing solution polishing

                           