Abrasive Wheels
Product Description
Cuting is the first step in material analysis, and the selection of the cutting machine and abrasive wheels must meet the geometric dimensions and material characteristics of the sample. TROJAN's cutting products make the cutting process simple, fast, and precise.
Perfect metallographic cutting should avoid thermal damage and deformation while maintaining the necessary precision and cutting speed. Hardness and ductlity are the two main factors when selecting abrasive wheels. The optimal choice depends on the material's size, hardness, ductility, and the equipment used.
TROJAN abrasive wheels feature a unique formula that ensures effective cooling and minimizes thermal damage. Additionally,their surface design prevents debris accumulation during cutting, making cleaning easier and keeping the workbench and cutting chamber clean.