We use first- and third-party cookies including other tracking technologies from third party publishers to give you the full functionality of our website, to customize your user experience, perform analytics and deliver personalized advertising on our websites, apps and newsletters across internet and via social media platforms. For that purpose, we collect information about user, browsing patterns and device.

By clicking "Accept All Cookies", you accept this, and agree that we share this information with third parties, such as our advertising partners. If you prefer, you can choose to continue with "Only Required Cookies". But keep in mind that blocking some types of cookies may impact how we can deliver tailored content that you might like.

For more information and to customize your options, click on "Cookie settings". If you want to learn more about cookies and why we use them, visit our Cookie Policy page at any time. Cookie Policy

Accept All Cookies Close

Metallographic Examination of Automotive Bearing Coatings

Metallographic cross-section analysis plays an important role in evaluating automotive bearing coatings. Microscopic examination helps assess coating thickness and continuity, nickel barrier layer integrity, and potential pores, inclusions, or cracks at material interfaces. Banding or interfacial defects within the coating can compromise structural integrity and become potential crack initiation sites or sources of delamination under cyclic loading. Reliable metallographic preparation helps identify coating defects, thickness variations, and bonding issues, supporting coating quality control and failure analysis.

Metallographic cross-section analysis of automotive bearing coatings showing coating thickness and material interfaces

Sample Preparation Procedure

Mounting

MT-1H BB2232 hot mounting compound.

Grinding & Polishing

Alpha-610 automatic grinder/polisher.

  1. Grinding: P400 MET-SP + water
  2. Fine grinding: POS + 9 μm PD-WT
  3. Coarse polishing: SC-JP + 3 μm PD-WT
  4. Final polishing: ZN-JP + 0.05 μm SO-A539
Metallographic micrograph showing the coating layer and steel backing interface in an automotive bearing sample

A well-prepared cross-section provides a reliable basis for evaluating coating integrity and bonding quality between the coating, alloy layer, and steel backing.

Detailed metallographic examination of automotive bearing coating interfaces showing microscopic features and defects
#AutomotiveMaterials #BearingCoatings #Metallography #FailureAnalysis #SamplePreparation #MaterialsCharacterization #TrojanMetallographic