Grinding is involved in many industries, whether it is the furniture industry or the automotive industry that people come into contact with in their lives, or the field of electronic appliances that involves higher precision and greater complexity, it plays an important role.
Grinding, as the name implies, is to grind and polish the surface of the sample to obtain a flat and smooth surface. In the field of metallography, it can provide better observation and analysis of the sample. So far, conventional sandpaper still has problems such as uneven particle size, easy shedding of abrasives, and low grinding efficiency, which leads to frequent replacement of sandpaper. In order to solve or alleviate the occurrence of the above problems, our company has launched a Trojan metallographic film sandpaper. Compared with traditional sandpaper, it is not only less prone to wrinkles, but also has improved grinding efficiency by at least 3-5 times. It greatly improves the service life of a single sandpaper and reduces frequent replacement.
The following is the data record of the comparison test between Trojan film sandpaper and conventional sandpaper (all test schemes are unified and consistent):




英语
西班牙语
德语