MA-2275 Mineral-filled Edge Retention Hot Mounting Resin
Product Description
Mineral filled melamine resin.
We use first- and third-party cookies including other tracking technologies from third party publishers to give you the full functionality of our website, to customize your user experience, perform analytics and deliver personalized advertising on our websites, apps and newsletters across internet and via social media platforms. For that purpose, we collect information about user, browsing patterns and device.
By clicking "Accept All Cookies", you accept this, and agree that we share this information with third parties, such as our advertising partners. If you prefer, you can choose to continue with "Only Required Cookies". But keep in mind that blocking some types of cookies may impact how we can deliver tailored content that you might like.
For more information and to customize your options, click on "Cookie settings". If you want to learn more about cookies and why we use them, visit our Cookie Policy page at any time. Cookie Policy
Product Description
Mineral filled melamine resin.
Features
Features: High hardness, good adhesion to sample surfaces, and excellent grinding and polishing performance.
Application: Suitable for medium-hard materials, such as standard hard alloys, general steels, aluminum, copper, and other materials.
Technical Parameters
|
Description |
Mineral-Filled Edge Retention Hot Mounting Resin |
|
Appearance |
Light Yellow Particles and White Powder |
|
Holding Time |
4-7 min |
|
Cooling Time |
5-8 min |
|
Cooling Rate |
Medium |
|
Heating Pressure |
150-300bar |
|
Heating Temperature |
150-180˚C |
|
Hardness (Shore D) |
92-95 |
Ordering Information
|
Order No: |
Description |
Package |
|
02.01.960 |
Yellow, Grit |
1kg |
|
02.01.965 |
Yellow, Grit |
4kg |
|
02.01.970 |
Yellow, Grit |
20 kg |