TJ 2800 Acrylic Resin
Product Description
Acrylic resin has good permeability and stable chemical properties. It is typically used for rapid curing or the preparation of a large number of samples.
We use first- and third-party cookies including other tracking technologies from third party publishers to give you the full functionality of our website, to customize your user experience, perform analytics and deliver personalized advertising on our websites, apps and newsletters across internet and via social media platforms. For that purpose, we collect information about user, browsing patterns and device.
By clicking "Accept All Cookies", you accept this, and agree that we share this information with third parties, such as our advertising partners. If you prefer, you can choose to continue with "Only Required Cookies". But keep in mind that blocking some types of cookies may impact how we can deliver tailored content that you might like.
For more information and to customize your options, click on "Cookie settings". If you want to learn more about cookies and why we use them, visit our Cookie Policy page at any time. Cookie Policy
Product Description
Acrylic resin has good permeability and stable chemical properties. It is typically used for rapid curing or the preparation of a large number of samples.
Features
Features: Semi-transparent, good edge retention, and low shrinkage rate. It performs better with a cold mounting press.
Curing time: 8-10 minutes
Technical Parameters
|
Material |
TJ 2800 |
|
Part A |
Resin, Powder |
|
Part B |
Hardener, Liquid |
|
A : B ( w/w ) |
10:5 |
|
Mixing Time |
2-4 min |
|
Curing Time |
8-10 min |
|
Peak Temperature |
85 ° C |
|
Hardness |
82 |
|
Edge Retention |
Better |
*Φ30mm mold, under room temperature conditions of 20-25℃.
*The Trojan DSV10 solvent can be used to dissolve resin that has already cured.
Ordering Information
|
Order No: |
Description |
Package |
|
02.03.511 |
White, Resin, Powder |
1 kg |
|
02.03.512 |
Hardener, Liquid |
1000 ml |